Default I'll offer two thoughts

1. 40 feet isn't really very far away from the salt water, particularly in a blow.

2. I wouldn't trust powder coating in that application. The smallest crack or chip will let moisture (and salt) get to the underlying metal and then the whole business will peel off. By contrast, a good galvanizing job will, to some extent, be self-healing.

Jim Fulton